By neo2122 - 8/21/2019 3:02:18 AM
From the XC110 datasheet,
CURED MECHANICAL PROPERTIES Tests performed on XC110-C331T2-210(1250) laminate cured out-ofautoclave Property Test Standard Units Result Compressive strength BS EN ISO 14126 : 1999 MPa 483 Tensile strength BS EN ISO 527-4 : 1997 MPa 521 Tensile modulus BS EN ISO 527-4 : 1997 GPa 55.1 Flexural strength BS EN ISO 14125 : 1998 MPa 777 Flexural modulus BS EN ISO 14125 : 1998 GPa 46.7 Interlaminar shear strength BS EN 2563 : 1997 MPa 64.7 Tg Onset (DMA) ASTM 1-0003 Issue 3 °C 121 Tg Peak (DMA) ASTM 1-0003 Issue 3 °C 135
I understand the standards relating to the tests are as specified. Can I have further information (ie. thickness, number of ply(s), method of cure, cure temp & duration, etc..) regarding the specimens sent for these tests?
|
By Warren (Staff) - 8/21/2019 9:44:54 AM
We do not have specific test token lay up schedule available. The test token sizes are specified in each BS/ISO standard and the lay up will be as required to meet the required thickness.
This is why the actual data is presented in units that are specifically dimensionless so they can be used for most situations.
|
|