Talk Composites - The Forum for Advanced Composites

Vacuum pump from ebay

http://www.talkcomposites.com/Topic33594.aspx

By Classicarbon - 8/20/2019 5:22:27 PM

I recently puchased vacuum pump from eBay and I was struggling to find adaptor for outlet end.It come out it's 7/16 some American standard tread. So if anyone will be interested this company got them:
https://burtonhydraulics.co.uk
So you can have 7/16 -1/4 adaptor