+xHi,
You could put some tape or similar on the back, then fill in from the front using filleting wax.  Press the wax down slightly so it slightly recesses and you should then see the vent outline on the mould and part surface giving you a line to cut to.
Aaa thought so,just mix the sides where to stick tape. Great thanks