By Jones - 7/30/2019 7:42:10 PM
Im looking into using silicone bags instead of the disposable nylon bags. mainly in order to deal with problems such as leaking bags, bridging, reducing consumables, as well as reducing the time it takes. Right now im still in school so doesn't have too much cash to throw around, I have therefore opted to go for brush on silicone bags. I have looked into using either Alan harpers starter kit or the ez brush silicone from smooth-on.
Mainly im looking inte you guys opinions regarding the subject as there is not alot of information out there apport from a few videos and articles but if feels like no-one is talking about it on forums and such.
what are you guys thoughts regarding: brush vs sprayed silicone and brands. distributing epoxy/resin. (all in one shot Alan Harper style, gravity fed/resin infusion or injecting with machine etc) sealing profiles. (on flange, routed grove, wax strips etc) flow distribution (morph runners, resin runners, Alan harpers REFLOW Flow Promoter, regular flowmesh, core or reinforcement with flow properties etc) just wanted to mainly get the discussion started and your experiences and opinions regarding it all.
|
By oekmont - 8/2/2019 8:55:39 AM
It's a matter of how thick your cavity is compared to the thickness of your layup when it's compressed to the maximum. Your layup should be less than 1,5 mm. So if you use 1,5 mm wax sheets, you should have a good flow speed. No need for a flow pattern. It will only get your part stuck to the upper mould. As long as you are not injecting 2min resins, you should get away without pressure injection.
|
|