By jamesw - 11/12/2012 3:55:19 PM				
            
                      
            I have built a large oven designed to run at temps of up to 70c,
  I am trying to pick a way to heat it, but wanted some advice on the flammability of epoxy resin fumes in an sealed environment, as am a little worried that a fan heaters' glowing element could cause an explosion risk...
  I know there's a thread on here with someone using a fan heater in a box, but I'm not sure if he uses for post cure only or also "wet" coating cure (I will be doing both)
  Thanks, James
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Jack.Strong - 11/14/2012 9:23:15 AM				
            
                      
            Could always use a fire retardent epoxy
  Alternatively if you search for a COSH form, or MSDS into epoxy you can find a risk assessment pdf which may contain useful information
           
		 | 			
		 
	
	
						
		 	
		
	 |