By Lukasz - 7/25/2019 8:42:19 AM
Good morning I have a problem .After finishing the bonding of the all holes in canoe I had some resin left, so I smeared the whole canoe and the next day I poured water and come white surface appeared but not where I put new patches. What happened what is causing it How to get rid of it. Please help me
|
By Warren (Staff) - 7/29/2019 10:45:30 AM
Glad it worked out in the end. Moisture can cause havoc so it is well worth bearing that in mind in future.
|
|