By Caddyshack - 7/23/2019 3:53:01 PM				
            
                      
            Hi,
  I have a Renault Twizy electric car, it has 4 (ABS I think) Plastic mudguards that sit on the suspension so rise and fall with the wheel, they have heavy metal supports and reinforcement and I wanted to make Carbon replicas...is there any need to make a mould when I could add release agent etc, to the actual mudguard and lay the pre-preg on top? I know it would add a few mm to the dimensions but that would not matter.
  Note, I do not want to carbon cover them, I want a carbon lightweight alternative.
  I would aim to do the same with the front and rear grey plastic "bumpers".  If the weave finish was not perfect I would wrap them satin or gloss black.
  
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By scottracing - 7/24/2019 10:38:18 PM				
            
                      
            I know Chris at zero ev. He's helping out doing an upgraded twizzy battery pack.
           
		 | 			
		 
	
	
						
		 	
		
	 |