+xfantastic work, what materials did you use?
Thx buddy!
-Easy lease chemical release agent + Meguiar's #8 wax
-1st layer:200gm2 twill
2nd layer:300gm2 -+45° biaxial carbon fabric
For the first layer I used Aerofix3 adhesive spray for the better comsmetic result, between the first and second layer I used a cheaper one adhesive spray. There are 6 installation point on this part. On the frontside you can see that deep drillpoints. Those are strong enough, but the rear ones (the vertically part of the fender) need one more extra 300gm2 biaxial reinforcement.
-IN2 infusion epoxy
Hope I could help you!