By frankp2138 - 6/18/2019 9:10:04 AM
I have read the XC 130 data sheet, I am new to this material and would like to be advised by an expert opinion. I have to make a small component with many details (Bike frames), in autoclave. These are the times and temperatures of my way to cycle curing

|
By Warren (Staff) - 6/18/2019 2:53:12 PM
Looking at the data sheet that looks fine for 100C cure cycle with the added post cure. You could always do a lower temperature cycle if you find the resin needs more time to flow.
|
|