hi, I am new to epoxy and find it fascinating; thought I would say hello.
I have ordered the carbon fibre skinning starter kit and will be skinning a table top.
probably a dim question - applying the mix with a brush as on the video's must mean
getting through a lot of brushes; is there another way to apply the epoxy?
and; I can't find a video that shows how to fold at the corners, I have some ideas but
thought I would pose the question as I am here.
thank you in anticipation of help.
graham
By Warren (Staff) - 6/3/2019 11:55:32 AM

Welcome to the Forum!

There are quite a few skinning experts here on the forum who should be able to help you with your project. 

In terms of brushes, you can clean them in acetone after each use.

The corners may need a cut in the fabric to ensure the fabric does not crease up or lift.