By clueless - 5/29/2019 1:07:51 PM

Hi all, first off apologies if this is posted in the wrong area.

I'm looking for advice on repairing slight damage in two areas to a carbon fibre wheel, please keep in mind I really am clueless when it comes to this stuff! I understand from a quick google search that epoxy resin would be the best option, any help, advice and guidance very much appreciated!

Craig

a.
By clueless - 5/30/2019 12:45:40 PM

Rich (Staff) - 5/29/2019 4:09:29 PM
Given the small amount to repair as well, check out our Black Epoxy Repair Filler, we offer a small 100g pot and it has various filler materials to alter the viscosity and sandability as well as being quite fast curing. The other benefit being that it is coloured to match carbon quite well so you may be able to make a barely noticeable repair.

Already ordered, thanks again Smile