By ian.g - 5/13/2019 9:50:20 AM				
            
                      
            Hi I have some serious imperfections in my mould which will need filled.
  Using Gelcoat and wax works fine in small areas but I wondered if there was some other type of filler more suitable for larger surface imperfections - like a car body filler?
  I would be using the mould to make a part to make another decent mould from (I know!!) 
  Thanks
  
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By ian.g - 5/14/2019 2:13:19 PM				
            
                      
            Thanks - that had occurred to me because it will be much easier to sand off raised imperfections from the part rather than trying to infill the mould - so I think I will try to improve the mould a bit using gel coat and wax to ensure the part won’t have release issues then put the work into the new part to get a good ‘new’ mould.
  
           
		 | 			
		 
	
	
						
		 	
		
	 |