Talk Composites - The Forum for Advanced Composites

Semi-permanent release agent, wipe or spray?

http://www.talkcomposites.com/Topic32770.aspx

By FiveO - 5/5/2019 4:09:49 PM

Hi,

What produce better surface quality? I have tried wipe on method, but it leaves wipe marks and wet marks to some places. Can someone who sprays semi-permanent can talk about the difference from wiping. I am using Frekote.
By FiveO - 5/7/2019 9:34:19 AM

Lester Populaire - 5/6/2019 6:40:33 AM

try to wipe on and wipe off 15min later with a cloth that is barely wet with frekote and keep polishing. never used frekote but should work i assume. for things like this i like to use axel 832 which is really easy to apply. 

I can't do that, because my frekote vaporize in seconds and unevenly. But I think it's time to try other brand. 

But other thing is multiple coats. I was thinking, that if I put next wet coat on and wipe it off, doesn't it destroys the previous coat, because like frekote says not to touch the wet coat?