By demy182 - 4/19/2019 10:41:13 AM
do you think it is possible to build a surfboard with the infusion on both sides and a eps core inside?
|
By oekmont - 4/23/2019 11:24:14 AM
My foam is still exactly as before. Pressure is still at 8 mbar. Seems like not every foam, maybe even most foams can take it. Hardness is not a criteria, the foam I used is a wobbly as eps foam can get. I could quite easily crush it with my fingers.
|
|