By Kist - 4/14/2019 6:27:44 PM

I am new to using Glass Caste 50.

I was wondering what the rules are for use of resin on glass.

I have experimented on small piece of glass and it appears to be ok but the resin would be better if it was not so liquid is there a thickening agent? And should the glass have a primer on first?

I have tried using micro powders which are to translucent which others could I use to give a deeper a colour but still translucent ?

Hope I can do this as I have a project in mind 😊

Thank you for any advice

By Kist - 4/15/2019 6:35:58 PM

Thank you for this I will check out thickners and use more colour in the mix. Thanks again