Epoxy and ABS?

http://www.talkcomposites.com/Topic32509.aspx

By ian.g - 4/5/2019 1:47:53 AM

I want to use a ABS edge on my moulded Carbon fibre product - will the epoxy resin and the ABS bond ok and is there any danger of the ABS being melted by the resin?

Thanks

Ian
By SleepingAwake - 4/8/2019 7:37:12 AM

ian.g - 4/5/2019 7:02:37 PM
Thanks very much for your information. Could you please explain what the flame process does to the ABS - would a heat gun do the same job - I need to use a heat gun anyway to bend the ABS...

I'm not a chemist and not really qualified to elaborate more on what's going on exactly, but i understand that the surface is oxidizing. I have my doubts that the heat gun is enough heat as all the industrial settings i have seen used a torch to modify the surface. but this is typically something you want to make a quick test yourself anyway to test the process. so grab some ABS, a heat gun and a lighter and see how it goes.