By Davidbac - 3/2/2019 9:40:56 AM
Hello Can you explain the principles behind how to get a high gloss finish on the GC3 (Glasscast 3) After I have sanded down my surface moving down to sandpaper 2000 the surface is very Dull/matt then what do I do ? I am thinking I then polish using topfinish 2 and hard then medium then soft polishing pads,is this correct ??
Thanks David
|
By Warren (Staff) - 3/4/2019 11:14:09 AM
You can start with the NW1 polish from around 1500 grit then finish off with the TopFinish 2 for the final high gloss finish.
|
|