By 111mattin111 - 2/28/2019 7:32:41 AM
Hi what's the best way to get rid of this on my CF bonnet, how far does it have to be flat back to go?
|
By CmCarbon - 3/1/2019 7:13:37 PM
Try wet sanding it untill it's gone and then clearcoat it with a good 2k clear.
|
|