 Hello, i need to seal all of this bark, but only can do 30cm each 12hours, because if i turn the wood, the resin drop to the floor, because the resin is very liquid.
 Can i accelerate the drying time adding temp or adding any thing??
 
 Thanks.
 David
 
 
 
 
  
 
 
   |  
		| By Rich (Staff) - 2/4/2019 2:41:40 PM 
 The other option may be to use a different resin, depending on the effect that you're trying to achieve. Which resin is this and are you just coating the sides?
 |  |