3mm Solid Rod =10.6g / metre
3mm(2mm) Tube = 6g / metre
5mm(3mm) Tube = 18g / metre
I hope this helps - The weights are listed under the specification tabs for each of the tubes/rods (for future reference).
Cheers... I should have looked harder... my bad
Del