Hi,
I am experiencing issues with particle (Aluminum oxide, Al2O3) agglomeration in epoxy systems. See Researchgate for more information:
https://www.researchgate.net/post/Which_is_the_best_way_to_prevent_the_agglomerations_of_Al2O3_nano_particles_into_polymer_during_the_production_stage
What particle treatment do you recommend to avoid agglomeration in epoxy systems?