By abhiggs - 1/5/2019 11:26:44 AM
I have a carbon fibre tiller (off a racing yacht) and the clear coat/lacquer is cloudy, chipped and flaking in places. In sanding it down with P800 is appears to be very thin and in places the surface become rough. I suspect I am through to the carbon fibre because when I wet it it stays dull. Should I strip off all the clear coat and give it a coat or two of XCR and if so will it still require a clear coat on top of that?
|
By Warren (Staff) - 1/17/2019 12:03:58 PM
If you suspect you have gone through to the fibres, which it sounds like you have, then a coat of XCR should certainly help. Once cured and flatted back and polished, you should get a good level of shine without needing an additional clear coat.
|
|