By David CHEN - 10/22/2012 2:13:23 AM				
            
                      
                    I am a newbie  in the  forum 
          I'd have some questions about wacuum bagging process         
          1 When do  I use perforated film or unperforated film as reslease film ? Is it none-perforated release film is used  for pre-preg vacuum bagging and perforated is used in wet lay-up process ?   Can I not use the reslease film because there is peel ply to remove the breather cloth , or can I just use perforated film to take the place of the peel ply ?
           2How can I  make smoothness on both sides of the  composite laminate plates used for testing  ?
            3  If   I want to produce composite laminate plates of different thicknesses using different number of layers of carbon fiber woven roving , how could I make sure the fiber content is about the same?
            Thanks for your reply
 
  
           
		 | 			
		 
	
	
						
		 	
		
	 |