Talk Composites - The Forum for Advanced Composites

Guitar Mould!

http://www.talkcomposites.com/Topic31427.aspx

By ian.g - 12/29/2018 11:08:36 AM

I would like to make a clone of my guitar in CF using my guitar as a mould. Do you think I do this without destroying the finish on my guitar?

Thanks

By Hanaldo - 12/29/2018 2:05:49 PM

It's so so difficult to say, theres so many types of paint that aren't compatible with fibreglassing resins. When in doubt, it's definitely safer to say it isnt compatible and use PVA release agent.