By Carbon Tuner - 10/16/2012 4:23:34 PM
Well I want to make a hood, I don't think to many of my customers care about what the bottom looks like too much. I was wondering if anyone had any ideas where I could just reinforce the hood with something universal?
Instead of making the 2 molds I'd like to just make the top and figure out a way to make the other side without another giant mold.
|
By NikCFC - 10/30/2012 10:04:52 AM
You can just use 6mm-8mm foam core on the top part of the hood to add stifness. That's how I make hoods for race cars. Stiff & light.
|
|