By f1rob - 11/9/2018 8:37:28 AM
Has anyone used a good release for silicone on silicone ??? The release supplied by the silicone supplier is a spray wax,something similar to waxoil ! It works but with lots of transfer to the new part and the mould I am doing has lots of deep 4mm wide channels so very hard to spray a "light coat" as the TDS says. Have heard of mac wax ? From mould life I belive ? But this is also wax based and sounds very similar to what I'm using at the minute. Does anyone know of any others ??? Used a system years ago,but have no idea what it was which was a clear fine mist and invisible once sprayed or the part demoulded
|
By Hanaldo - 11/10/2018 7:55:33 AM
The Stoner range are quite good and have minimal transfer.
|
|