Hi,

I have been trying to build some small composite parts using either f.glass and or carbon 2/2 twill or a combination of both.

The basic part is approx. 3" long and has a deep 0.6" cavity about 0.3" wide in the shape of a Doug out canoe.

I have tried to a vaccuum bag setup pulling 20" inches but was getting voids and bridging... Etc.

Having just watched the videos should I try VIP and get a pump that can pull 29-30 inches or continue down my current path which is Making a mould (female/male).  I am getting close to getting it right, but it has taken several goes with a cnc machine.



Next question is do you have a product that can be used like gel coat on small parts to get a good finish, currently using 3/4 fglass as the first layer but still get some pin holes.  Just don't want to go to all the effort to setup a dump gun for a 3" part.





Thanks in advance,



Adrian
Australia
By al010964 - 10/25/2012 9:28:14 AM

Hi All,

My part is a servo cover not a spat, similar shape but more aggressive curves.

I have chatted to Adam (wyowindoworks) previously, I didn't think of him as not sure how much VIP he does.

But a good idea never the less.