By Carbon Tuner - 10/4/2012 12:27:31 PM				
            
                      
            Hey everyone. 
   
  I have made a few parts that just have some minor pinholing in the corner, I polished the part but now I have the white polish in these pinholes. 
   
  Whats the easiest way to get it out, any ideas for filling the pinholes? not really looking to fill with epoxy then sand again.
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By fgayford - 11/10/2012 2:25:15 AM				
            
                      
            On another forum a few guys said they just used black shoe polish. It fills the holes black and makes them disappear.