By Haggis50 - 9/15/2018 8:46:28 AM
Can Melamine sheet be used as a mould for GlassCast Epoxy resin? If so, do you need to use a release agent as well?
|
By scottracing - 9/17/2018 5:50:34 PM
We use melamine boards as flanges when making prepreg tooling. Ive used both wax and chemical release on it.
|
|