Talk Composites - The Forum for Advanced Composites

Whats the mould made from in this carbon making tutorial ?

http://www.talkcomposites.com/Topic2933.aspx

By mickthecat - 9/28/2012 6:37:18 PM

As above. Can anyone tell me what its made from ?

http://www.google.co.uk/url?sa=t&rct=j&q=carbonmods&source=web&cd=9&cad=rja&sqi=2&ved=0CEUQtwIwCA&url=http%3A%2F%2Fwww.youtube.com%2Fwatch%3Fv%3DIAdVO8Rkv6c&ei=LOBlUL70K-Hs0gXq3YCwDA&usg=AFQjCNH1R26NHSaRH36y0WVDDBxQZIc5rg

Cheers

Mick
By Matt (Staff) - 10/2/2012 10:52:58 AM

Hi Mick,

Yes, that one is GRP; it's made from the Uni-Mould mould making system as we were experimenting with pre-pregs back when we made that laminating video (5 years ago!) and wanted the mould to (a) be compatible with epoxy and (b) be able to take temperature for pre-pregs.