By Shaun - 9/2/2018 1:09:56 PM
Hi Guys, first time playing with CF. I am a designer and 3d printing enthusiast.
Im going to have a crack skinning the inside of these prototype velocity stacks that are going to live on a sprint car. Obviously this is a fiddly curvature, I was thinking for layup I should approach it in 3 or 4 pie sections with the 2x2 twill I've got here. I was just assuming any less than 3 fabric sections per layer and it would start trashing the weave etc.
Thoughts? (just one stack at a time not as a whole)
2" base dia 4.5" across the top.
Thanks in advance for any replies !
|
By Shaun - 9/2/2018 11:29:12 PM
thanks again oekmont, im feeling more confident now 
this is the profile i kindly borrowed from a volvo penta engineers design study

|
|