By cvasilliou - 9/1/2018 8:41:25 AM
what material/s should i use to create a mould and then applying pre-preg to that mould.i imagine a foam of high temperature resistance cause in the process we have to cure it in high temperatures right?any other ideas?i want the material to be as cheap as possible.
|
By Hanaldo - 9/7/2018 1:19:27 AM
Yes, you could use the epoxy tooling board - do you need that level of accuracy though?
Why not just make a fibreglass mould? By far the most straightforward and cheapest method.
|
|