By BMac - 8/12/2018 6:28:03 PM
I have tried 3 times to put a final coat on my carbon skinned parts but I still keep getting air bubbles and pitholes. I have sanded, cleaned, 3-1 mix and all new brushes etc. I'm using the xcr resin. Below are the photos. Can anyone help.

|
By BMac - 8/13/2018 7:03:28 AM
240 dry
|
|