By Andrew Murdoch - 7/23/2018 8:17:32 AM
I have made a wooden table top and in the centre I have cut out a rectangular shape ( 29cm by 60cm ) and glued down small ceramic tiles. The height of the inlay from top of the tiles to the level of table top is 8mm. Can I use GlassCast 30 to fill in the inlay and coat the table top all in one go, or do I need to use GlasCast 50 to fill in the inlay and pour Glasscast 30 over that and the rest of the table top.
|
By Warren (Staff) - 7/24/2018 12:08:33 PM
Yes the GlassCast 3 is ideal for Beer bottle tops. The 3 generally applies to the typical thickness of the resin coat over the top of the objects which for beer top tables etc is around 3mm. So filling the gaps up is fine.
|
|