By sclarke81 - 7/21/2018 6:50:27 PM
Hi, During my project I managed to spill some drops of XCR Epoxy Coating Resin on my smooth sandstone slabs in my garden. Do you have any advice on how to remove it? Thanks, Stephen
|
By Hanaldo - 7/22/2018 4:31:35 AM
Chipping it off will be the only way. You can try to weaken the bond by burning it with a blow torch.
|
|