By twissta - 9/16/2012 10:16:43 AM				
            
                      
            After resin infusion, and the part is cured at room temp. do you have to cure it in an autoclave to insure that the part doesn't deform, delaminate or get soft in the sun....?
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren - 10/3/2012 7:36:18 PM				
            
                      
            A postcure will improve the properties of the end product.  
  Also once the infusion has been done, if you dont postcure then in reality there will still be resin that hasnt fully cured hence the need for a postcure at elevated temperature.
  Sure eventually it will fully cure itself but you are looking at months in the cool british climate.
           
		 | 			
		 
	
	
						
		 	
		
	 |