By ants87ss - 6/30/2018 7:01:59 PM
First Id like to say Hello from The US. I have gained a bunch of knowledge from this forum as well as the EasyComposites YouTube videos. Thank You!
I am going to mold my first part, a trim panel off a Ford Mustang. As you see below, there is a few burrs around the holes where an emblem once mounted. My question is, do i sand the area around the holes smooth, leave the area dull, add clay and proceed with gel coat? Or do I just fill with clay, lay out gelcoat and sand the gelcoat smooth after cure? This panel is plastic, and I do not believe it is painted. I am concerned that I will not be able to buff the area if it is sanded. I was wondering what would be easier, sand the mold afterwards or just sand before. Thanks a ton in advance
|
By Hanaldo - 7/27/2018 2:05:11 AM
You still need to hold it in the correct position initially. The expansion of the foam will want to twist it if it can.
|
|