By Alanh - 6/25/2018 11:49:12 AM
I’m trying to find a supplier of HDU board for chip carving which is normally done on European Lime wood this generally runs at a density around 540 to 590kg per m3 because of a bit of arthritis I need something around 250kg/m3, there are such products available in the states but they are too expensive for me to import, be grateful if anyone could point me in the right direction
|
By Alanh - 6/26/2018 6:34:29 PM
New material arrived 18 hours after placing the order and it’s spot on, it’s approximately 1/2 to 2/3 the density of the average kiln dried Lime wood and it carves beautifully with crisp sharp definition to the cuts.
Thank you Hanaldo
|
|