By Jim Sutherland - 6/13/2018 5:14:18 PM

Hi,

I saw your video on repairing a composite kayak recently (How to repair a damaged composite Kayak).  Looks like my surf ski (a Stellar S18S) has the same material of construction as your video example.  Would appreciate it if you could list the specific repair items from the video so I could order...including the carbon/Kevlar fabric, release film and epoxy/hardener combo used (item numbers if possible to make my ordering easier Smile)

Thanks very much,

Jim Sutherland 
By Matt (Staff) - 6/14/2018 10:09:50 AM

Hanaldo - 6/14/2018 12:45:41 AM
Have a look here, all the materials are listed on the right:

http://easycomposites.co.uk/#!/composites-tutorials/kayak-repair-tutorial

Spot on Martin, thanks; that page lists all the products.