By bubba kodi - 6/7/2018 9:29:12 AM
i want to do a river table i have a idea on different colours and glow in the dark power question is if i use glow in the dark power can i mix the glow in the dark power into a solid colour or is it just with tinting pigments
|
By Warren (Staff) - 6/8/2018 8:16:08 AM
Although you can mix the pigment into a solid colour, realistically you will get a limited glowing effect as only the powder that ends up on the surface would be visible and hence glow. So in practice I would recommend using the tinting pigments with the glow powders.
|
|