By Martin.P - 5/20/2018 8:21:39 PM
I have been making a few wooden plates on the CNC machine & using glasscast to fill any cracks, knot holes & splits in the wood as it is food safe. Works really well but now I have been asked by a Restaurant if I could make them some live edge steak platters from wood that they can provide that has a significance to either them or the Restaurant ( not sure which but not important lol).
Problem is that although Glasscast is food safe I have been told by someone that it is not dishwasher safe & since these will be washed in an industrial dishwasher it's quite possibly not going to be an option.
So my question for the experts, Is what I have been told about it not being dishwasher safe true & if it is does anyone know of a clear food safe resin that is dishwasher safe.
|
By Warren (Staff) - 5/23/2018 8:09:09 AM
The ArtResin should fill small cracks and splits just fine. It is not quite as runny as GlassCast but it does still have a long pot life so will soak in where it needs to before it sets.
|
|