Dear Sirs,
can you recommend a resin which can be used to attach a thermocouple (PTFE insulated or fibreglass insulated) to the inside of a brass bolt, which can withstand temperatures up to 250degC? I'm looking for a very small amount, so ideally a small bottle should be enough if it's available of course.
Regards, Tom
|
By dsc - 8/22/2012 10:43:20 AM
Hi guys,
thanks for the information. I've now decided to use a 1.5mm TC probe and a Swagelok tube adapter to hold it in place. Solves all my problems.
Thanks, Tom
|
|