By pedcrist - 8/11/2012 5:32:57 PM				
            
                      
            Hello,
  I have a doubt, where do i place dthe connectors using this 2 materials?
  This way??
 
  
  Or this way?
 
  
 
  
  Or another one??
  the realese film that i have is unperforated.
  Thanks,
  Pedro
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By pedcrist - 8/12/2012 7:40:23 PM				
            
                      
            Hello,
  I´going to explain what i´m doing: it´s a front motorcicle fender, and i want both sides shinny as the piece come out of the mould, so that´s why i´m using release film and brether cloth.
  I thought i could infuse it, but it seems i can´t, i was mixing the processes.
  I think that i´ve already seen this way, but now i´m not sure.
  Hereupon, what is the best way to do it?
  Thanks,
  Pedro
           
		 | 			
		 
	
	
						
		 	
		
	 |