Hi all,

Is there any esy way to reduce the curing temeprature and heat soak of curing resin in a high volume to surface area layup?

Cheers,

Dave.
By oekmont - 5/5/2018 3:07:43 PM

The usual countermeasures are
1st: using slower resin systems
2nd: try to achieve a high fibre content