By Kurt Halkier - 4/6/2018 11:45:56 AM
Are there any time limits for achieving a good bond strengt when adding a second layer of IN2 Infusion Resin, to a surface made earlier with the same type Resin, and should the hardened resin be treated or sanded first?
|
By Warren (Staff) - 4/6/2018 4:00:56 PM
If it has gone past the firm but tacky stage, then as long as you give the surface a good key with sand paper and a thorough clean then there is no real time limit.
|
|