Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Hand Layup
Post cured cleaning
http://www.talkcomposites.com/Topic25595.aspx
By benji
-
4/4/2018 9:00:39 PM
I recently finish a part but the part of the piece facing the mould is still sticky. Not quite sure why.
I start to "brush" it slightly with acetone but not quite sure it's the right thing to do.