By SeanS - 3/20/2018 12:49:57 PM
Hi everyone Im looking for a 180 deg C curing out of autoclave pre-preg, anyone know where I could get that in small quantities? In small quantities is the key thing here, few metres needed just. Tried the usual companies, any tips appreciated, even europe thanks
|
By scottracing - 3/26/2018 9:51:57 PM
most 180 degree cure prepregs are aerospace spec and requyire the use of an autoclave, you could look at a lower temp curing material and post cure up to 180degrees?
|
|