By Lonebandit - 3/16/2018 9:19:58 AM
Ok so as many I got inspired by the recent video I watched on how they created a carbon fiber bonnet with what looked like an oem bonnet. Ok now yea simple as easy peezy. What I would like to do is create a same thing but with my oem fender now I just can’t wrap my head around how would I get the shape on where the bolts go. Should it be a 1 piece or 2 piece mold? Again I want to use exact same method gentleman used on the video. Thanks talkC community.....2012 DODGE CHALLENGER fenders
|
By Warren (Staff) - 3/16/2018 5:37:54 PM
Most non-closure panels are single skin to start with. Only closure panels need double skins.
|
|