By Enric Ibars - 3/8/2018 10:29:26 PM
I am new from Spain, trying to build a resin infusion longboard with carbon fiber and bamboo. I feel easy composites webpage and videos very well explained so, I said to myself..."I am goig to try it" I was googling for information and I got this forum, is very good to have it so we can share and learn from other composite enthusiasts. Than you
|
By Enric Ibars - 3/9/2018 10:16:30 AM
+xHi Enric, welcome to the forum. A few people on here have experience with making boards so it is a good resource. If you haven't already seen it, then I would recommend you watch our video on infusing a long board. We used recycled pallet wood, some natural fibres and a more environmentally friendly epoxy resin. If you haven't seen it then the video is here: Resin Infused Skateboard Using Carbon Fibre, Flax and Bio Resin Yes I seen it, is wonderful. I have been trying for a long time with prepregs with good results but it was brick due to very thin areas, and I made another one with fiberglass that is still is running. Thank you
|
|