By GreyArea - 2/22/2018 9:20:44 PM
I was wondering which (if any) of your resins would make a normal piece of 80gsm A4 copier paper the most transparent if it was used to make a thin sheet...just a single piece of paper and enough resin to soak into it. I thought maybe one of the laminating resins was the obvious choice, but thought I'd ask...
|
By oekmont - 2/23/2018 5:55:38 AM
paper usually only gets opaque. but there are copy fleeces commercially available, wich you can print on, but wich become almost glass glass clear, once wetted out with epoxy.
|
|